TyphimuriumBiofilm kelvin probe force microscopy BFO MagneticForce TriGlycineSulphate DNA pinpoint mode solar_cell Scanning_Thermal_Microscopy Boundary Floppy ChemicalCompound SiliconeOxide tip_bias_mode OpticalWaveguides CeNSE_IISc Sulfur AmplitudeModulation sputter GlassTemp Melt IndiumTinOxide 2d_materials P3HT Hole Graphene Polystyrene ULCA PinPointMode polymeric_arrays oxide_layer Growth DiffractiveOpticalElements AAO Biology
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LPDE
Spincast layer of PS/LDPE blend on Si. Signal change by thermal conductivity difference.
Scanning Conditions
- System: NX10
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512