CalciumHydroxyapatite PVAC Friction LateralForceMicroscopy PolycrystallineFerroelectricBCZT Tapping UnivMaryland ContactModeDot Ni81Fe19 Ito Tungsten Pvdf MagneticForceMicroscopy mechanical property HanyangUniv HexagonalBN HighAspect cannabidiol silicon_carbide HighAcpectRatio DNAProtein Piezoelectric TransitionMetal hetero_structure Al2O3 layers BiasMode Microchannel PMNPT PolyStylene Wang SICM Ucl MolybdenumDisulfide neodymium_magnets
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 3μm×3μm, 1μm×1μm
- Scan Rate: 0.4Hz, 1Hz
- Pixel: 512×512, 512×512