Ito Celebration Electrical&Electronics Phase molecular_beam BismuthFerrite Switching SPMLabs Growth Sic RedBloodCell thermal_conductivity Polyvinylidene_fluoride semifluorinated_alkane TemperatureControlledAFM TransitionMetal MultiLayerCeramicCapacitor Chemical Vapor Deposition fifber norganic FFM Al2O3 Ceramics ConductingPolymer Flake Conducting PvdfBead Cobalt-dopedIronOxide LiftMode HiVacuum Implant Film cannabinoid Hexylthiophene PANI
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256