Mfm FFM CrystalGrowing Chloroform dielectric_trench ThermalConductivity SurfaceChange Titanate ChemicalCompound PECurve MechanicalProperties Resistance Nanotechnology KevlarFiber Transparent Electronics Polyvinylidene_fluoride strontiu_titanate Ucl Formamidinium_lead_iodide fifber Pinpoint PFM Magnetostrictive Solar alkanes Tungsten Co/Cr/Pt DIWafer PatternedSapphireSubstrat self_assembly nanomechanical PolyStylene Aluminium_Oxide BTO UnivMaryland
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ER 316L Stainless Steel
The ferrite MFM phase has a striped appearance due to its ferromagnetic behavior, while the paramagnetic austenite phase shows a uniform appearance.
Scanning Conditions
- System: NX20
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm
- Scan Mode: AM-KPFM, MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.3Hz
- Pixel Size: 512 × 512
- Lift height: 30nm