VortexCore IVSpectroscopy Hydroxyapatite ElectroChemical Materials epitaxy Writing Barium_titanate Epoxy Subhajjit Lanthanum_aluminate Ito kelvin probe force microscopy SmallScan hard_disk Foil Regensburg cross section Force-distance UnivOfMaryland DiffractiveOpticalElements gallium_nitride Polyurethane self_assembly Yeditepe_University LogAmplifier Nanofiber PS_PVAC Pvdf Molybdenum PiezoelectricForceMicroscopy Wafer YszSubstrate TriGlycineSulphate Conduct
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferroelectric 2L-hBN
Scanning Conditions
- System : FX40
- Sample bias: 0.25 V, 0.8 V
- Scan Mode: C-AFM
- Scan Rate : 8 Hz
- Scan Size : 1.5μm×1.5μm
- Pixel Size : 256×256