Chemical Vapor Deposition rubber HanyangUniv IMT_Bucharest NeodymiumMagnets Alloy pulsed_laser_deposition Hexatriacontane Pipette PetruPoni_Institute Techcomp Metal-organicComplex ShenYang Al2O3 MetalCompound Edwin Transparent nanomechanical AlkaneFilm Fiber Singapore small_scan Bmp Nanostructure UnivMaryland MESA structure CntFilm Pinpoint PFM Hexacontane Fe_film VinylAlcohol high_resolution HfO2 Switching Ceramic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Polymer (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: NCHR
- Scan Size:1μm×1μm
- Scan Rate: 1Hz
- Pixel: 256 × 256
- Scan Mode: Tapping
- Cantilever: NCHR
- Scan Size:1μm×1μm
- Scan Rate: 1Hz
- Pixel: 256 × 256