Polyethylene Platinum Bismuth LateralForceMicroscopy OpticalWaveguides DIWafer Silicon SRAM TemperatureControlledAFM HardDiskMedia Fiber Neodymium TappingMode Topography Protein hetero_structure Tape MechanicalProperty Lateral_Force_Microscopy GaN MagneticArray Cobalt H-BN PVAP3HT VinylAlcohol PhaseChange Indent KevlarFiber PolycrystallineFerroelectricBCZT Metal AIN ScanningKelvinProbeMicroscopy TransitionMetal Inorganic Zagreb
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512