hydrocarbon IIT-chennai Titanate TipBiasMode MagneticArray Beads HardDisk Magnetic Force Microscopy Bmp semifluorinated alkane WS2 molecular_beam light_emission Etch DataStorage Liquid TemperatureControl thermal_conductivity DLaTGS PolyvinylAcetate IndiumTinOxide AdhesionForce Tin sulfide SiliconOxide Pvdf I-VSpectroscopy Potential Austenite LaAlO3 CeramicCapacitor Polyvinylidene Christmas blended polymers kelvin probe force microscopy IcelandSpar
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HfO2 into Indium Tin Oxide Film
ITO film on 1% HfO2-doped Yttria-stabilized Zirconia (001) orientation grown by pulsed laser deposition. Surface segregation of HfO2 into ITO film.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz))
- Scan Size: 10μm×10μm,5μm×5μm
- Scan Rate: 0.6Hz, 1Hz
- Pixel Size: 256 × 256, 256 x 256