Dr.JurekSadowski Pinpoint PFM Polyethylene plastics Ni81Fe19 Hafnia CVD Bismuth ScanningIon-ConductanceMicroscopy FAPbI3 TemperatureControlledAFM DiffractiveOpticalElements Pzt graphene_hybrid LateralForce UnivMaryland Ca10(PO4)6(OH)2 self_healing Hair conductive BiasMode StrontiuTitanate Tape PVAC CaMnO3 MagneticArray CntFilm Permalloy Leakage align GaP self-assembly University_of_Regensburg Conducting Wonseok
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
CTa2B12H12 Nanosheet
Scanning Conditions
- System : XE7
- Scan Mode: Contact, LFM
- Scan Rate : 0.5 Hz
- Scan Size : 6.5μm×6.5μm
- Pixel Size : 256×256
- Cantilever : RTESPA-150 (k=5N/m, f=150kHz)