FAFailureAnlaysis flakes CarbonNanotube AIN HfO2 CancerCell WWafer Cobalt-dopedIronOxide Iron Spincast Heat Cell LiIonBattery Vac Pores Metal SiliconCrystal Optical Gallium_Arsenide Biology HanyangUniv Epoxy Alkane StyreneBeads HumanHair PiezoelectricForceMicroscopy HighResolution BiFeO3 India PFM CrystalGrowing TemperatureControllerAFM FailureAnlaysis LithiumNiobate Nanopattern
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
NCA of Li-ion battery (2/2)
Scanning Conditions
- System : NX-Hivac
- Sample bias: 1 V
- Scan Mode: SSRM
- Scan Rate : 0.25Hz
- Scan Size : 15μm×15μm
- Pixel Size : 256×256
- Cantilever : AD-40-AS (k=40N/m, f=200kHz)