lift_mode MolecularSelfAssembly F14H20 RedBloodCell cannabinoid CastIron amplitude_modulation NusEce ThinFilm small_scan PVA Polymer BoronNitride frequency_modulation YttriaStabilizedZirconia Fet GaAs IIT-chennai OpticalWaveguides TipBiasMode Tungsten Piezoresponse LithiumNiobate VinylAlcohol HydroGel Memory Step NUSNNI strontiu_titanate ImideMonomer align pulsed_laser_deposition Barium_titanate Polytetrafluoroethylene Epoxy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Perovskite coated on glass with Palladium electrodes
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : All 0.4 Hz
- Scan Size : 40μm×40μm
- Pixel Size : All 256×256
- Cantilever : NSC36 Pt C(k=0.6N/m, f=65kHz)