Change Lattice Inorganic Filter Reading Mfm Edwin FAPbI3 Chungnam_National_University NCM\ MeltingPoint dielectric trench Global_Comm Barium_titanate Yttria_stabilized_Zirconia Composition NCM Metal Cross-section SiWafer blended polymers Thermal Sidewall MolybdenumDisulfide polyvinyl acetate MfmAmplitude PolyStylene epitaxy DNAProtein PpLdpe CuFoil CrossSection TungstenThinFilmDeposition cannabinoid fluoroalkane
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcite surface change in Ca(OH)2
Scanning Conditions
- System: NX20
- Scan Mode: Universal liquid cell, Contact mode
- Cantilever: BL-AC40TS
- Scan Size: 45μm×45μm, 0.5μm×0.5μm
- Scan Rate: 3Hz
- Sample: Iceland spar (calcite)
- React Solution Ca(OH)2
- Pixel: 512 × 256, 256 × 256
- Scan Mode: Universal liquid cell, Contact mode
- Cantilever: BL-AC40TS
- Scan Size: 45μm×45μm, 0.5μm×0.5μm
- Scan Rate: 3Hz
- Sample: Iceland spar (calcite)
- React Solution Ca(OH)2
- Pixel: 512 × 256, 256 × 256