StrontiuTitanate Scratch Blend Wonseok FrictionalForceMicroscopy Sperm Ananth OrganicSemiconductor Gold Chemical_Vapor_Deposition UnivCollegeLondon Water Chromium molecules Flake Silver piezoelectric force microscopy thermoplastic_elastomers ScanningTunnelingMicroscopy conductive Beads Hole 2dMaterials Conductance ThermalConductivity Wang HexacontaneFilm PolymerBlend Stiffness Inorganic Mosfet Yeditepe_University Topography Temperature Composition
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PVDF beads
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: Arrow UHF (f=2000kHz)
- Scan Size: 30μm×30μm, 10μm×10μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 512×512, 512×512
- Scan Mode: Non-contact
- Cantilever: Arrow UHF (f=2000kHz)
- Scan Size: 30μm×30μm, 10μm×10μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 512×512, 512×512