FailureAnalysis Wonseok Sulfur Chromium ScanningIon-ConductanceMicroscopy CastIron molecule Nanofiber Boron Tapping FFM Polypropylene GlassTemp CeNSE_IISc light_emitting Resistance C36H74 DNAProtein Fet Cross-section epitaxy SingleLayer ContactModeDot Galfenol AtomicSteps Magnetic Force Microscopy Hysteresys Heating piezoelectric force microscopy BiasMode MembraneFilter Blood Mechinical Praseodymium Cobalt
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Stitched image of chiplet
Scanning Conditions
- System : NX-Wafer
- Scan Mode: Non-contact
- Scan Rate : 0.5 Hz
- Scan Size : 100μm×100μm for single image (200μm×200μm stitched image)
- Pixel Size : 512×128 for single image
- Cantilever : OMCL-AC240TS (k=2N/m, f=70kHz)