medical SPMLabs AdhesionEnergy HDD PVAP3HT Pzt Led Vacuum pinpoint mode Filter ScanningSpreadingResistanceMicroscopy Self-assembledMonolayer molecular_self_assembly BiasMode 2d_materials membrane MetalCompound Ceramic Ceramics Sio2 Bismuth Sic SetpointMode Gold Inorganic PvdfBead Photovoltaics Spincast CeNSE_IISc Nanostructure ForceMapping Magnets Scanning_Thermal_Microscopy CancerCell molecular_beam
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG
Scanning Conditions
- System : FX40
- Scan Mode: Sideband, AM KPFM
- Scan Rate : 0.55 Hz
- Scan Size : 10μm×10μm
- Pixel Size : 256×256
- Cantilever : NSC36 Cr-Au C (k=0.6N/m, f=65kHz)