norganic Nickel StrontiuTitanate LightEmission Ferroelectric biocompatible DeoxyribonucleicAcid Steps Semiconductor single_layer CastIron dichalcogenide Self-assembledMonolayer SrO BaTiO3 Materials Hole Deposition Calcium SelfAssembly contact Chromium STO light_emission LiquidCell PhaseTransition Laser Pipette CarbonNanotube Hysteresys Alloy Topography Tin disulfide CNT IMT_Bucharest
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
2L-MoS₂ (2/3)
Scanning Conditions
- System : FX40
- Sample bias: 0.5 V
- Scan Mode: C-AFM, LFM
- Scan Rate : 12 Hz
- Scan Size : 1μm×1μm
- Pixel Size : 512×512
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)