Sphere Chemical_Vapor_Deposition Electical&Electronics Inorganic LiIonBattery CompactDisk MESA structure Vac ForceVolumeMapping Solution Piranha LogAmplifier Lateral GaN neodymium_magnets Wafer fluoroaalkane PinpointNanomechanicalMode GlassTemp HighAspect fifber ElectroChemical NUS_Physics StyreneBeads FM-KPFM TiO2 SKKU Gong Korea Defects Ito Current Phenanthrene Bmp Optic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Semiconductor device, Failure analysis
Scanning Conditions
- System: NX10
- Scan Mode: Conductive AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 11μm×11μm
- Scan Rate: 1Hz
- Pixel: 512×512
- Sample bias: -0.5V