Layer cannabis Ananth Piezoelectric SiliconCrystal NUS_NNI_Nanocore vertical_PFM Vanadate Leakage ScanningIon-ConductanceMicroscopy Organic TemperatureControllerAFM Piranha Thermal Memory India Electrode Molybdenum_disulfide Oxide Polyvinylidene_fluoride NiFe graphene_hybrid light_emitting VinylAlcohol Patterns SicMosfet 2dMaterials IISCBangalore I-VSpectroscopy ThinFilm Ptfe blended polymers Cross-section hard_disk Aluminium_Oxide
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single-crystal SrTiO3(001) after Annealing
Single-crystal SrTiO3(001) after 1h annealing at 1000°C in air. Formation of steps and terraces, and assembly at the nanoscale of SrO and TiO2 chemical terminations.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256
- Scan Mode: LFM
- Cantilever: qpBioAC CB1 (k=0.02N/m, f=110kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 1Hz
- Pixel Size: 256 × 256