Flake HafniumDioxide DataStorage FrictionalForce Laser Styrene CrystalGrowing hydrocarbon PUR TemperatureControl Ram BariumTitanate aluminum_nitride Force-distance Sperm ForceVolumeImage VortexCore MolecularSelfAssembly OpticalWaveguide alkanes SKKU LeakageCurrent CastIron molecule PvdfFilm Polytetrafluoroethylene hard_disk_media vertical_PFM doped rubber PANI NiFe OrganicCompound C36H74 MultiLayerCeramicCapacitor
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferromagnetic Nanobars Array
Ferromagnetic nanobars arranged on a Penrose P2 tiling. The Permalloy (Ni81Fe19) nanobars are 810 nm and 500 nm long. The width and thickness of a nanobar amount to about 120 nm and 25 nm, respectively.
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 7μm×7μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Lift height: 85nm
- Scan Mode: MFM