Dental PhaseTransition Genetic LightEmission ito_film PVAC MfmPhase Insulator mechanical property kelvin probe force microscopy Molybdenum OxideLayer Vac Dimethicone Phosphide mfm_amplitude Monisha Polymer Copolymer Boron PMNPT Magnetostrictive thermoplastic_elastomers Scratch NCM\ lithography Neodymium Polytetrafluoroethylene block_copolymer ElectroChemical Calcite NCM University_of_Regensburg SmalScan C36H74
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BTO
Scanning Conditions
- System: XE7
- Scan Mode: DC-EFM(Vertical)
- Cantilever: ElectriMulti75G (k=3N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.2Hz
- Pixel: 256×256
- Sample Bias: 0V
- Tip Bias: 1V ac
- Scan Mode: DC-EFM(Vertical)
- Cantilever: ElectriMulti75G (k=3N/m, f=75kHz)
- Scan Size: 20μm×20μm
- Scan Rate: 0.2Hz
- Pixel: 256×256
- Sample Bias: 0V
- Tip Bias: 1V ac