Polyvinylidene bias_mode Anneal Phenanthrene Vac Pores non_contact Thermal phase_change ReflexLens PetruPoni_Institute FuelCell ForceMapping MolybdenumDisulfide HexagonalBoronNitride MoS2 Mechanical&nanotechnology UTEM Reduction Blood PFM TemperatureControllerStage Tin disulfide Bismuth 2-vinylpyridine graphene_hybrid BiasMode SingleCrystal Transparent Molybdenum CBD GlassTemp cooling FrictionalForceMicroscopy Neodymium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Styrene beads
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 2μm×2μm
- Scan Rate: 0.5Hz
- Pixel: 512×512