IISCBangalore OrganicSemiconductor Epoxy FailureAnlaysis PinpointPFM Al2O3 BloodCell Mechanical&nanotechnology ThermalDetectors Electrical&Electronics Blood Scanning_Thermal_Microscopy Cobalt silicon_oxide Water graphene_hybrid ForceVolume TriGlycineSulphate BiasMode Vac SingleLayer SetpointMode Topography Chemical Vapor Deposition SrTiO3 Wang strontiu_titanate CNT Wonseok InsulatorFilm StainlessSteel LiquidCell Titanate CopperFoil TemperatureControl
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Graphene on hBN
Scanning Conditions
- System : FX40
- Sample bias: 1 V
- Scan Mode: C-AFM
- Scan Rate : 25 Hz for 25 nm2, 10 Hz for 50 nm2
- Scan Size : 25nm2×25nm2
- Pixel Size : 128×128 for 25 nm2, 256×256 for nm2
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)