Magnetic Force Microscopy PrCurve Scratch Galfenol Polypropylene HBN TCS PinPointMode HexagonalBN Writing block_copolymer WPlug StyreneBeads ElectroDeposition Barium_titanate StrontiuTitanate Sulfur Mosfet Floppy BismuthVanadate NeodymiumMagnets Dimethicone Polytetrafluoroethylene Steps Mfm BismuthFerrite Worcester_Polytechnic_Institute Electrode BloodCell Hydroxyapatite LiquidImaging Celebration Calcium Molybdenum_disulfide Gallium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferroelectric superlattices in 2L-hBN (0°)
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : All 0.3 Hz
- Scan Size : 3μm×3μm, 4μm×4μm
- Pixel Size : All 512×512
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)