EvatecAG Boundary hetero_structure Vanadate DeoxyribonucleicAcid Metal-organicComplex ContactModeDot C36H74 Tin sulfide Sapphire IISCBangalore suspended_graphene MeltingPoint ThermalConductivity InorganicCompound HardDiskMedia Electronics Laser mechanical property Biofilm EFMAmplitude WS2 Typhimurium FrictionalForceMicroscopy SurfaceChange Spincast Indent Piezo Electrical&Electronics SingleLayer Pattern EFM LeakageCurrent Zagreb Ito
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2 (2/2)
Scanning Conditions
- System: NX10
- Scan Mode: KPFM
- Cantilever: NSC36Cr-Au(k=1N/m, f=90kHz)
- Scan Size: 30μm×30μm,10μm×10μm
- Scan Rate: 0.1Hz
- Pixel: 512×1024