MolybdenumDisulfide Plug FailureAnlaysis Optoelectronic suspended_graphene MultiLayerCeramicCapacitor LowDensityPolyethylene temp_control MfmPhase InsulatorFilm ScanningKelvinProbeMicroscopy Regensburg LaAlO3 block_copolymer Defects CVD HighResolution Fet Anneal Tin sulfide LiquidCell BTO thermal_conductivity SKKU PolycrystallineFerroelectricBCZT Change ScanningThermalMicroscopy BreastCancerCell Nanopattern Domain Zhi medical AM_KPFM Beads EFMAmplitude
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512