LateralForceMicroscopy DomainSwitching OrganicSemiconductor PVAP3HT domain_switching Gong contact #Materials FloppyDisk NeodymiumMagnets HumanHair dielectric trench StyreneBeads ScanningTunnelingMicroscopy DentalProsthesis CrAu MagneticForceMicroscopy Hafnia AtomicSteps Organic NUS_NNI_Nanocore Chungnam_National_University Sadowski PhaseTransition C36H74 NTU Vac BreastCancerCell IIT-chennai pulsed_laser_deposition Sperm CuParticle SSRM Genetic MultiferroicMaterials
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Calcium Hydroxyapatite Crystal growing
HA crystal grows according to the annealing time. From 24hrs, the crystal becomes clearly.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 1μm×1μm
- Scan Rate: 0.17Hz
- Pixel: 512×256