FM_KPFM small_scan self-assembled_monolayer plastics Semiconductor Nickel NCM\ Au111 HardDiskMedia Zhi Subhajjit NTU FrictionalForce PMNPT HexacontaneFilm PtfeMembrane AtomicSteps Inorganic_Compound Floppy INSP BaTiO3 fe_nd_b vertical_PFM FM_SKPM TungstenDeposition Collagen Mapping ForceMapping Monisha Annealing Mechanical oxide_layer FastScan SFAs Beads
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Co/Cr/Pt
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×512
- Lift height: 40nm
- Scan Mode: MFM
- Cantilever: PPP-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 1Hz
- Pixel: 512×512
- Lift height: 40nm