AdhesionEnergy #EC Vinylpyridine ShenYang cannabis Phthalocyanine SingleCrystal WPlug Magnetic MagneticArray norganic PetruPoni ReflexLens doped Typhimurium CompactDisk Edwin Tapping Vortex BoronNitride SurfaceOxidation ScanningKelvinProbeMicroscopy small_scan TCS hetero_structure OpticalModulator DeoxyribonucleicAcid PANI Varistor StrontiuTitanate Biology Implant FrequencyModulation Dental FailureAnalysis
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Magnetic Vortex Core (Ni-Fe alloy)
Scanning Conditions
- System: NX10
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm
- Scan Mode: MFM
- Cantilever: LM-MFMR (k=2.8N/m, f=75kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.2Hz
- Pixel: 1024×1024
- Lift Height: 80nm