SingleCrystal kelvin probe force microscopy LiNbO3 WPlug Stiffness Hydroxyapatite molecular_beam chemical_compound IRDetector Tungsten Polyvinylidene_fluoride VortexCore NiFe FailureAnalysis Holes rubber PetruPoni_Institute Thermoplastic_polyurethane Mapping Cell Oxide SiliconeOxide HighAspect Ceramic Change self-assembled_monolayer Anneal Ni81Fe19 Polyvinylidene Perovskite CuParticle Pinpoint PFM Worcester_Polytechnic_Institute ForceVolumeImage BismuthFerrite
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BiVO4 on treated YSZ substrate
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.36Hz
- Pixel: 256×256