#EC Workfunction ElectroChemical bias_mode self_healing Monisha PinpointNanomechanicalMode Optoelectronic CNT Oxidation LiftMode Fe_film Ferroelectric SRAM SICM Device PMNPT strontiu_titanate Magnets Croatia Epoxy MLCC Barium_titanate BTO Hair UTEM Array Nickel MagneticPhase PhaseTransition SKKU TriGlycineSulphate Polymer MembraneFilter WPlug
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG
Scanning Conditions
- System : FX40
- Scan Mode: Sideband, AM KPFM
- Scan Rate : 0.55 Hz
- Scan Size : 10μm×10μm
- Pixel Size : 256×256
- Cantilever : NSC36 Cr-Au C (k=0.6N/m, f=65kHz)