Chemical Vapor Deposition Gallium food Organic atomic_steps FFM Tin sulfide Silver Yeditepe_University Hole Conductance norganic PinpointPFM CopperFoil Bismuth LiquidImaging Chromium SelfAssembly Pores Mechanical&nanotechnology frequency_modulation AM-KPFM 3-hexylthiophene GaN PolycrystallineFerroelectricBCZT block_copolymer Layer LiIonBattery ElectroDeposition LogAmplifier FM-KPFM semifluorinated_alkane Heat layers temp_control
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LPDE
Spincast layer of PS/LDPE blend on Si. Signal change by thermal conductivity difference.
Scanning Conditions
- System: NX10
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512
- Scan Mode: SThM
- Cantilever: NanoThermal Probe
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 256 × 512