Litho self_assembly LiBattery WWafer Photovoltaics Grain Genetic Ito OpticalModulator Array TemperatureControllerAFM PDMS AM-KPFM PpLdpe Polyvinylidene mechanical_property Battery Conduct MolecularSelfAssembly Blood Hexylthiophene CuFoil Yeditepe MagneticPhase Silicon hetero_structure NUS Phase Oxide OrganicSemiconductor TungstenDeposition CHRYSALIS_INC SFAs FrictionForce fifber
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PS/LDPE
Spincast layer of PS/LDPE blend on Si.
Scanning Conditions
- System: NX10
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512
- Scan Mode: LFM
- Cantilever: BL-AC40TS (k=0.09N/m, f=110kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 1Hz
- Pixel Size: 512 × 512