CancerCell ScanningIon-ConductanceMicroscopy Wildtype ScanningTunnelingMicroscopy Biofilm fluorocarbon PvdfFilm TemperatureControlledAFM Alkane ForceVolumeImage SetpointMode PolycrystallineFerroelectricBCZT Gold Modulus ThermalProperties Pinpoint Tin sulfide ScanningThermalMicroscopy Pores PolyvinylAcetate Fujian Patterns Friction HighResolution PhaseImaging ferromagnetic PyroelectricDetector Global_Comm Chungnam_National_University layers MolybdenumDisulfide BFO LithiumNiobate NUSNNI Solution
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
MoS2
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 25μm×25μm
- Scan Rate: 0.8Hz
- Pixel Size: 512 × 256
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 25μm×25μm
- Scan Rate: 0.8Hz
- Pixel Size: 512 × 256