BismuthFerrite Hexatriacontane China cannabis BlockCopolymer Aluminum mechanical property Metal-organicComplex SiliconOxide PolymerPatterns PhaseChange PinpointNanomechanicalMode SingleCrystal Bmp Butterfly HardDiskMedia CP-AFM tip_bias_mode polyvinyl acetate Insulator SiWafer Lateral_Force_Microscopy HiVacuum Piezo FrictionalForce StrontiuTitanate CBD neodymium_magnets BFO Holes NusEce HumanHair Gong molecular_beam Phthalocyanine
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Composite Barium Titanate
PFM Quad color is overlaid on 3D surface morphology.
Scanning Conditions
- System: NX10
- Scan Mode: PFM
- Cantilever: PPP-ContScPt (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 256 × 256
- Scan Mode: PFM
- Cantilever: PPP-ContScPt (k=0.2N/m, f=25kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.3Hz
- Pixel Size: 256 × 256