Typhimurium Ferroelectric Hafnium_dioxide GaP TungstenDeposition WS2 Composition Materials Formamidinium_lead_iodide SrO 2-vinylpyridine Optoelectonics light_emission Croatia Fluoride CancerCell Nanostructure LiftHeight LateralForceMicroscopy semifluorinated alkane Blend kelvin probe force microscopy CuFoil ForceMapping ScanningThermalMicroscopy OpticalWaveguide Magnetostrictive MLCC Yeditepe WWafer PVAC Indent H-BN HBN Bacterium
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Formamidinium Lead Iodide FAPbI3 Perovskite Film
FAPbI3 is an organic-inorganic hybrid perovskite material for nowadays high efficiency perovskite solar cell.
Scanning Conditions
- System: NX10
- Scan Mode: Conductive AFM
- Cantilever: CDT-NCHR (k=80N/m, f=400kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256