Silver Force-distance Mobile TPU Liquid Chromium University_of_Regensburg fluorocarbon AM-KPFM PANI Chloroform ForceMapping ScanningTunnelingMicroscopy PDMS non_contact SFAs lithography Phase AdhesionForce Sic Composition CP-AFM Treatment NusEce CarbonNanotube Yeditepe Vortex Leakage Adhesive Ito ElectrostaticForceMicroscopy high_resolution Polydimethylsiloxane Wang Lattice
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
HOPG
Scanning Conditions
- System: NX20
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256
- Scan Mode: FM-KPFM
- Cantilever: qpBioAC AuCB1 (k=0.3N/m, f=90kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.5Hz
- Pixel Size: 512 × 256