Organic RedBloodCell TiO2 CuParticle Typhimurium layers Wildtype LiIonBattery Implant INSPParis Calcite Lateral H-BN thermal_property Piezoelectric Chungnam_National_University AtomicLayer atomic_steps Cobalt Ferrite nanomechanical Current Optic HexagonalBoronNitride SiliconCrystal ElectrostaticForceMicroscopy BariumTitanate HardDisk TransitionMetal LifeScience ScanningThermalMicroscopy Yttria_stabilized_Zirconia Pipette HexagonalBN PFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Suspended single-layer Graphene
Single-layer Graphene is suspended on microchannels fabricated on Si/SiO2 substrate.
Scanning Conditions
- System: NX20
- Scan Mode: Non-contact
- Cantilever: Access-NC (k=113N/m, f=330kHz)
- Scan Size: 40μm×40μm
- Scan Rate: 0.4Hz
- Pixel Size: 256 × 256