molecules Display LeakageCurrent Roughness Spain Butterfly MfmAmplitude LowDensityPolyethylene Mfm oxide_layer TriGlycineSulphate Wonseok LMF ferromagnetic Gold Self-assembledMonolayer dielectric trench IIT-chennai Scanning_Thermal_Microscopy Mosfet neodymium_magnets nanomechanical Water contact Nanostructure FuelCell HardDisk medical amplitude_modulation ReflexLens Al2O3 Techcomp MonoLayer Chemical Vapor Deposition CaMnO3
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Self-assembly of Semi-fluorinated Alkanes
Domains formed by the self-assembly of semi-fluorinated alkanes deposited as a monolayer on the surface of the water. The monolayer was compressed before being transferred onto a silicon substrate. Each domain includes about 4000 molecules. The domains were easily detached from the substrate with tapping mode because the molecules were very loosely attached to the substrate. Only Non-contact mode could achieve this result.
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: PPP-FMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 2Hz
- Pixel Size: 500 × 500
- Scan Mode: Non-contact
- Cantilever: PPP-FMR (k=2.8N/m, f=75kHz)
- Scan Size: 1μm×1μm, 0.5μm×0.5μm, 0.2μm×0.2μm
- Scan Rate: 2Hz
- Pixel Size: 500 × 500