Indent aluminum_nitride NeodymiumMagnets ForceMapping AtomicSteps #EC CalciumHydroxide PrCurve Gallium_Arsenide HOPG MechanicalProperties Oxide self_assembly strontiu_titanate Alloy Polydimethylsiloxane HardDisk Sphere lift_mode AlkaneFilm LiquidImaging Fluoride Liquid Water C36H74 Reduction PolymerBlend Monisha OpticalWaveguides fluorocarbon PetruPoni contact Chrome Polystyrene Adhesion
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
PDMS liquid crystal
Scanning Conditions
- System: NX10
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×512
- Scan Mode: Tapping
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 15μm×15μm
- Scan Rate: 0.5Hz
- Pixel: 512×512