self-assembly Liquid Wonseok nanomechanical cross section SelfAssembly Wildtype sputter GaAs Biofilm Heat multi_layer self-assembled_monolayer Tape ScanningIon-ConductanceMicroscopy ScanningSpreadingResistanceMicroscopy Grain ContactModeDot BlockCopolymer CuFoil HDD light_emitting small_scan Ananth Sio2 DNA SurfaceOxidation HardDisk thermal_property temperature controller AFM Zagreb HiVacuum dielectric_trench Magnetic Force Microscopy CBD
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li ion battery electrode
Scanning Conditions
- System: NX-Hivac
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm, 5μm×5μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 4096×2048, 512×512