C60H122 Bacteria BiasMode Co/Cr/Pt Holes ConductiveAFM Ferrite Lift MolecularSelfAssembly Optic BiFeO3 Permalloy LiNbO3 Croatia FM-KPFM LateralPFM Edwin Reduction PVA PECurve PolyStylene Yttria_stabilized_Zirconia HexagonalBN medical TiO2 Jason TemperatureControl FM_SKPM VortexCore Sadowski LowDensityPolyethylene Bismuth InorganicCompound Magnetostrictive Workfunction
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
DNA, DNA Protein
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact in Air
- Cantilever: ACTA (k=40N/m, f=300kHz)
- Scan Size: 5μm×5μm, 1μm×1μm
- Scan Rate: 0.5Hz, 0.8Hz
- Pixel: 256×256, 256×256