FM_KPFM Heating AtomicSteps Bio Fluoride Styrene sputter FrictionalForce Anneal LiquidImaging non_contact Resistance semifluorinated_alkanes Collagen MechanicalProperties Composite vertical_PFM Polyimide PMNPT PetruPoni_Institute aluminum_nitride MeltingPoint MagneticArray Defects Temasek_Lab Transparent ScanningTunnelingMicroscopy SRAM Switching FuelCell TungstenDeposition silicon_oxide CBD Pipette VerticalPFM
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Ferroelectric 2L-hBN
Scanning Conditions
- System : FX40
- Sample bias: 0.25 V, 0.8 V
- Scan Mode: C-AFM
- Scan Rate : 8 Hz
- Scan Size : 1.5μm×1.5μm
- Pixel Size : 256×256
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)