FrictionalForceMicroscopy frequency_modulation Self-assembledMonolayer LateralForceMicroscopy Polyethylene Gong Metal-organicComplex Polyvinylidene_fluoride OpticalWaveguide light_emission PvdfBead Glass Fendb SThM Dr.JurekSadowski mechanical property BCZT Chemical_Vapor_Deposition CuParticle Ito Co/Cr/Pt UTEM Silver Gallium LiNbO3 Vac PFM self_healing Defect Permalloy LiBattery OrganicSemiconductor TiO2 Praseodymium norganic
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
NCA of Li-ion battery (1/2)
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : 0.25Hz
- Scan Size : 15μm×15μm
- Pixel Size : 512×512
- Cantilever : PPP-FMR (k=2.8N/m, f=75kHz)