LiftHeight Spincast self_healing PatternedSapphireSubstrat light_emitting TyphimuriumBiofilm Tungsten LateralForceMicroscopy PolymerBlend EFM norganic Stiffness Silicon Permalloy Tapping Fluoride Boundary TungstenThinFilmDeposition IVSpectroscopy CrossSection ForceVolume Oxide Materials RedBloodCell Austenite dichalcogenide HexacontaneFilm fluoroaalkane 2d_materials SetpointMode DiffractiveOpticalElements CuFoil Defects StyreneBeads layers
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Strainded MoS₂ on Si
Scanning Conditions
- System : FX40
- Scan Mode: Sideband KPFM
- Scan Rate : 0.15Hz
- Scan Size : 50μm×13μm
- Pixel Size : 2048×1024
- Cantilever : ElectricMulti75-G (k=3N/m, f=75kHz)