conductive Resistance Plug LightEmiting Ferrite Boundary MeltingPoint Growth nanomechanical SolarCell Vacuum UnivOfMaryland NUS_Physics Polyethylene Tin sulfide Phthalocyanine Temperature mfm_amplitude Nanotechnology MechanicalProperty HighAcpectRatio norganic Sic neodymium_magnets Galfenol BreastCancerCell BFO temp_control Ptfe Biofilm lift_mode LiftMode FastScan LateralForce atomic_layer
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
GaN on Si epi film
Scanning Conditions
- System : NX20
- Scan Mode: Non-contact
- Scan Rate : All 2 Hz
- Scan Size : 5µm2, 5µm2
- Pixel Size : ALL 512×512
- Cantilever : OMCL-AC160TS (k=26N/m, f=300kHz)