cannabis dielectric_trench Ca10(PO4)6(OH)2 WPlug Liquid PANI Hole Bio self-assembled_monolayer Electrical&Electronics Anneal TungstenDeposition Leakage molecular_beam LifeScience SurfaceOxidation Conductive AFM Styrene Permalloy NUS molecular_self_assembly molecule Memory ElectroDeposition Neodymium sputter Sic Zagreb block_copolymer ForceDistanceSpectroscopy Pzt HafniumDioxide silicon_oxide Annealed FastScan
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Single layer Graphene film on Cu foil
Scanning Conditions
- System: XE7
- Scan Mode: FM-KPFM
- Cantilever: NSC36C Cr-Au (k=0.6N/m, f=65kHz)
- Scan Size: 5μm×5μm
- Scan Rate: 0.5Hz
- Pixel: 256×256