Epoxy HiVacuum PolymerBlend #Materials Annealing GlassTemp ThinFilm Grain Electical&Electronics light_emission Vac ConductingPolymer Butterfly DOE temperature controller AFM Sic temp_control Temperature DeflectionOptics Bacterium Laser AIN Cobalt GaAs Alloy CrystalGrowing Force-distance Gallium_Arsenide blended polymers AtomicLayer CHRYSALIS_INC Fluoride Sio2 FloppyDisk I-VSpectroscopy
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Hard Disk Media
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: SSS-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.3μm×0.3μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256
- Scan Mode: Non-contact
- Cantilever: SSS-NCHR (k=42N/m, f=300kHz)
- Scan Size: 1μm×1μm, 0.3μm×0.3μm
- Scan Rate: 0.5Hz, 1Hz
- Pixel Size: 512×512, 256×256