amplitude_modulation Sadowski PrCurve Led Korea Thermal ScanningTunnelingMicroscopy high_resolution Yttria_stabilized_Zirconia polyvinyl acetate mechanical_property Modulus semifluorinated_alkane Silicon Graphene Tapping PinPointMode C60H122 LeakageCurrent ForceVolume Stiffness BCZT Ito Piranha ContactMode semifluorinated alkane TemperatureControl multi_layer AM_KPFM Pattern Temperature SurfaceOxidation UnivCollegeLondon Austenite WPlug
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
ITO glass
Scanning Conditions
- System: NX10
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512
- Scan Mode: CP-AFM
- Cantilever: CDT-Contr (k=0.5N/m, f=20kHz)
- Scan Size: 20μm×20μm, 1μm×1μm
- Scan Rate: 0.2Hz, 0.5Hz
- Pixel: 512×512, 512×512