atomic_steps Gallium_Arsenide solar_cell FrictionForce Dental Growth LifeScience Inorganic SetpointMode Non-ContactMode Polytetrafluoroethylene graphene_hybrid Regensburg ForceVolumeImage TCS CastIron Temperature Dopped StainlessSteel UTEM VerticalPFM Ceramics BiasMode PrCurve CrystalGrowing TiO2 Granada Sphere LateralPFM Cross-section ULCA OpticalWaveguide Solar Gallium MLCC
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
Li ion battery electrode
Scanning Conditions
- System: NX-Hivac
- Scan Mode: SSRM
- Cantilever: CDT-NCHR (k=80 N/m)
- Scan Size: 50μm×50μm, 5μm×5μm
- Scan Rate: 1Hz, 1Hz
- Pixel: 4096×2048, 512×512