IndiumTinOxide Silver norganic OrganicCompound Thermoplastic_polyurethane Wildtype Co/Cr/Pt SAM self_healing SoftSample polyvinyl acetate AM_KPFM Zagreb Dr.JurekSadowski TPU Sidewall atomic_layer PMNPT Alkane OpticalModulator GlassTemperature Bacteria AM-KPFM Treatment SetpointMode Ram TemperatureControl CeramicCapacitor multi_layer CalciumHydroxyapatite ferromagnetic PhthalocyaninePraseodymium Hafnium_dioxide MagneticPhase LateralForce
Report image
If you found this image unacceptable, please let us know. We will review your report and take action if we determine this image is really unacceptable.
BiVO4 on treated YSZ substrate
Scanning Conditions
- System: NX10
- Scan Mode: Non-contact
- Cantilever: AC160TS (k=26N/m, f=300kHz)
- Scan Size: 10μm×10μm
- Scan Rate: 0.36Hz
- Pixel: 256×256